Park Electrochemical Nelco® NX9270 PTFE Laminate, Woven-Glass Reinforced

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Park Electrochemical Corp.
Trade Name Nelco®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Park Electrochemical Nelco® NX9270 PTFE Laminate, Woven-Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminate system the material of choice for lowest loss, high frequency applications.Key Features and Benefits:Complete spectrum of controlled dielectric constantsEnhanced N9000 IM materials availableConsistent QualityOptimized N9000 PTFE processingApplications/Qualifications:Cellular Base Station AntennasWireless CommunicationsPower AmplifiersDual Band Hi Power Passive CircuitsAutomotive ApplicationsDigital/Microwave Hybrid Multilayer PCB AssembliesMillimeter Wave ComponentsTelecommunicationsInformation provided by Park Electrochemical Corp.
Physical Properties Metric English Comments
Specific Gravity 2.23 g/cc
2.23 g/cc
ASTM D792A
Water Absorption <= 0.020 %
<= 0.020 %
IPC-TM-650.2.6.2.1
Mechanical Properties Metric English Comments
Flexural Strength 68.9 MPa
9990 psi
Crosswise; IPC-TM-650.2.4.4
82.7 MPa
12000 psi
Lengthwise; IPC-TM-650.2.4.4
Peel Strength 2.312 kN/m
13.19 pli
after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8
2.33 kN/m
13.3 pli
18, 35, and 70µm copper; IPC-TM-650.2.4.8
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C
13.9 µin/in-°F
X; IPC-TM-650.2.4.41
35.03 µm/m-°C
19.46 µin/in-°F
Y; IPC-TM-650.2.4.41
260.21 µm/m-°C
144.56 µin/in-°F
Z; IPC-TM-650.2.4.41
Thermal Conductivity 0.272 W/m-K
1.89 BTU-in/hr-ft²-°F
ASTM E1225
Flammability, UL94 V-0
V-0
IPC-TM-650.2.3.10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IPC-TM-650.2.5.17
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IPC-TM-650.2.5.17
Dielectric Constant 2.36 - 2.74

@Frequency 1.00e+10 Hz
2.36 - 2.74

@Frequency 1.00e+10 Hz
IPC-TM-650.2.5.5.5
Dielectric Breakdown 50000 V
50000 V
IPC-TM-650.2.5.6
Dissipation Factor 0.0020

@Frequency 1.00e+10 Hz
0.0020

@Frequency 1.00e+10 Hz
IPC-TM-650.2.5.5.5
Arc Resistance 180 sec
180 sec
ASTM D495
Descriptive Properties Value Comments
Passive Intermodulation Formulation Availability Yes
Passive Intermodulation Performance (dBc) -155