| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
| Filler Content | 20 % | 20 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 29.96 MPa | 4346 psi | perpendicular; ASTM D638 |
| 34.21 MPa | 4962 psi | parallel; ASTM D638 | |
| Elongation at Break | 52.7 % | 52.7 % | parallel; ASTM D638 |
| 74.1 % | 74.1 % | perpendicular; ASTM D638 | |
| Flexural Modulus | 1.03 GPa | 150 ksi | perpendicular; ASTM D790 |
| 1.88 GPa | 273 ksi | parallel; ASTM D790 | |
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
| Dart Drop, Total Energy | 2.504 J | 1.847 ft-lb | Max Load; ASTM D3763 |
| 12.65 J | 9.330 ft-lb | ASTM D3763 | |
| Impact Test | 6.50 J | 4.79 ft-lb | Energy at Max load; ASTM D3763 |
| 20.4 J | 15.0 ft-lb | Total Energy; ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 48.1 µm/m-°C @Temperature -40.0 °C |
26.7 µin/in-°F @Temperature -40.0 °F |
ASTM D696 |
| 52.0 µm/m-°C @Temperature 66.1 °C |
28.9 µin/in-°F @Temperature 151 °F |
ASTM D696 | |
| 55.1 µm/m-°C @Temperature 121 °C |
30.6 µin/in-°F @Temperature 250 °F |
ASTM D696 | |
| CTE, linear, Transverse to Flow | 128 µm/m-°C @Temperature -40.0 °C |
71.3 µin/in-°F @Temperature -40.0 °F |
ASTM D696 |
| 141 µm/m-°C @Temperature 66.1 °C |
78.2 µin/in-°F @Temperature 151 °F |
ASTM D696 | |
| 147 µm/m-°C @Temperature 121 °C |
81.8 µin/in-°F @Temperature 250 °F |
ASTM D696 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | ASTM D648 |