Material Notes:
Monex is an expanded monel foil of uniform thickness (0.5mm or 0.75mm available) which is manufactured to give a large number of contact points per cm². It can be supplied with a filler of silicone or as plain foil, typical EMC performance is the same for either option. The filled variant will give an effective environmental sea whilst the unfilled variant provides EMC only. For best performance mating surfaces should have a tolerance of not more than 0.05mmSpecifications: Monel Foil – QQ-N-281bSilicone - ZZ-R-765-CL2 GR50Information provided by P & P Technology
Mechanical Properties Metric English Comments
Compression Set 1.0 %

@Pressure 0.345 MPa
1.0 %

@Pressure 50.0 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Silicone filled
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Silicone filled
Electrical Properties Metric English Comments
Shielding Effectiveness 42 dB

@Frequency 1.00e+10 Hz
42 dB

@Frequency 1.00e+10 Hz
P-Field
52 dB

@Frequency 10000 Hz
52 dB

@Frequency 10000 Hz
H-Field
68 dB

@Frequency 100000 Hz
68 dB

@Frequency 100000 Hz
H-Field
84 dB

@Frequency 1.00e+9 Hz
84 dB

@Frequency 1.00e+9 Hz
P-Field
88 dB

@Frequency 1.00e+6 Hz
88 dB

@Frequency 1.00e+6 Hz
H-Field
100 dB

@Frequency 4.00e+8 Hz
100 dB

@Frequency 4.00e+8 Hz
P-Field
>= 100 dB

@Frequency 1.00e+6 Hz
>= 100 dB

@Frequency 1.00e+6 Hz
E-Field
>= 100 dB

@Frequency 1.00e+7 Hz
>= 100 dB

@Frequency 1.00e+7 Hz
E-Field
>= 100 dB

@Frequency 1.00e+8 Hz
>= 100 dB

@Frequency 1.00e+8 Hz
E-Field
Descriptive Properties Value Comments
Closing Force 50-75 psi