Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 88 dB @Frequency 1.00e+6 Hz |
88 dB @Frequency 1.00e+6 Hz |
H-Field |
P & P Technology Monex Expanded Monel Foil Monex is an expanded monel foil of uniform thickness (0.5mm or 0.75mm available) which is manufactured to give a large number of contact points per cm². It can be supplied with a filler of silicon.. |
|||
Shielding Effectiveness | 88 dB @Frequency 1.00e+10 Hz |
88 dB @Frequency 1.00e+10 Hz |
26 in. x 26 in. test panel; TP08 Modified |
Parker Chomerics CHO-SHIELD® 2056 Conductive Coating CHO-SHIELD® 2054 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo.. |
|||
Shielding Effectiveness | 88 dB @Frequency 1.00e+9 Hz |
88 dB @Frequency 1.00e+9 Hz |
4mm x 6mm |
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t.. |
|||
Shielding Effectiveness | 88 dB @Frequency 1.00e+10 Hz |
88 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit SC-Consil® 860 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Shielding Effectiveness | 88 dB @Frequency 1.00e+10 Hz |
88 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit SC-Consil® FR861 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Shielding Effectiveness | 88 dB @Frequency 1.00e+10 Hz |
88 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit SC-Consil® FR862 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Shielding Effectiveness | 88 dB @Frequency 1.00e+10 Hz |
88 dB @Frequency 1.00e+10 Hz |
3mm x 25.4mm |
Parker Chomerics SOFT-SHIELD® 4850 Multi-planar EMI Gasket Description: SOFT-SHIELD® 4850 represents the latest advancement in EMI shielding gaskets based on Multi-planar, Z-axis conductive foam technology. SS4850 is based on the unique integration of elec.. |
|||
Shielding Effectiveness | 88 dB @Frequency 1.00e+10 Hz |
88 dB @Frequency 1.00e+10 Hz |
5mm x 25.4mm |
Parker Chomerics SOFT-SHIELD® 4850 Multi-planar EMI Gasket Description: SOFT-SHIELD® 4850 represents the latest advancement in EMI shielding gaskets based on Multi-planar, Z-axis conductive foam technology. SS4850 is based on the unique integration of elec.. |