Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Pro® 3216 CUW BLK Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Pro®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 3216 CUW BLK Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Multi-Pro 3216 CUW BLK is well suited for resin furniture requiring high impact strength and stiffness at moderate cost.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792-91
Melt Flow 16 g/10 min
16 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 21.7 MPa
3150 psi
ASTM D638-95
Elongation at Break 160 %
160 %
ASTM D638-95
Flexural Strength 37.9 MPa
5500 psi
ASTM D790-95
Flexural Modulus 1.897 GPa
275.1 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256-93a
Gardner Impact 11.3 J
8.33 ft-lb
ASTM D5420-93
Optical Properties Metric English Comments
Gloss 50 %
50 %
ASTM D2457-90
Users viewing this material also viewed the following: