| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 43.1 - 103 MPa | 6260 - 15000 psi | Average value: 75.1 MPa Grade Count:7 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
|
|||
| Tensile Strength, Yield | 62.1 - 103 MPa | 9000 - 14900 psi | Average value: 81.0 MPa Grade Count:8 |
|
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum ..
|
|||
| Tensile Strength, Yield | 14.8 - 103 MPa | 2150 - 14900 psi | Average value: 46.3 MPa Grade Count:363 |
|
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
|
|||
| Tensile Strength, Yield | 30.0 - 103 MPa | 4350 - 14900 psi | Average value: 72.4 MPa Grade Count:24 |
|
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
|
|||
| Tensile Strength, Yield | 34.5 - 103 MPa | 5000 - 15000 psi | 0.2% offset |
|
Eagle Brass 210 Gilding Metal, Annealed
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi..
|
|||
| Tensile Strength, Yield | 30.0 - 103 MPa | 4350 - 15000 psi | Average value: 56.9 MPa Grade Count:15 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
|
|||
| Tensile Strength, Yield | 0.241 - 103 MPa | 35.0 - 15000 psi | Average value: 30.3 MPa Grade Count:43 |
|
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..
|
|||