Gouda Vuurvast CURAS 50 PD Moldable Refractory Material

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURAS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURAS 50 PD Moldable Refractory Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high strength over the full temperature range. The mechanical strength of this material develops after heating above 150°C.Remarks: The stated chemical composition and physical properties represent average values.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.20 - 2.30 g/cc
0.0795 - 0.0831 lb/in³
After drying at 110°C
Thermal Properties Metric English Comments
Thermal Conductivity 0.700 - 0.800 W/m-K

@Temperature 100 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.830 - 0.930 W/m-K

@Temperature 600 °C
5.76 - 6.45 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.960 - 1.06 W/m-K

@Temperature 1400 °C
6.66 - 7.36 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Shrinkage -2.00 - 2.00 %

@Temperature 1400 °C
-2.00 - 2.00 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 50 %
50 %
Fe2O3 2.0 %
2.0 %
SiO2 40 %
40 %
Descriptive Properties Value Comments
Bonding Type chemical/ceramic
Material Consumption per 1 m3 2200 kg
Mixing Water 9-11 liters
per 100 kgs dry material