Material Notes:
Description: Naxel™ PC40 is a 20 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Melt Flow 20 g/10 min
20 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.3 MPa
8750 psi
ASTM D638
Elongation at Break 88 %
88 %
ASTM D638
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
ASTM D648