Solvay Specialty Polymers Polidan® EC/51 Polyethylene, Crosslinked (XLPE)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Crosslinkable
Manufacturer Solvay Specialty Polymers
Trade Name Polidan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Polidan® EC/51 Polyethylene, Crosslinked (XLPE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flexible low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards complying: IEC 60502 XLPE, IEC 60092/351, CEI 18-16/351, BS 7655 GP8, VDE 0276 2XI1, HD 604 2XI1Features: Crosslinkable; Good Flexibility; Low Density; Low ToxicityUses: Low Voltage Insulation; Wire & Cable ApplicationsAdditional Properties: Change in Bend Test - IEC 60811 (150°C): No cracks; Collar Temperature - 170 to 190 °C; Head Temperature - 170 to 190 °C; Hot Set - IEC 60811 50 %; Hot Set - IEC 60811 0.0 %; Insulation Resistance Constant - IEC 60502 (20°C): 15000 Mohm·km; Insulation Resistance Constant - IEC 60502 (90°C): 10000 Mohm·km; Water Absorption - IEC 60811 (100°C): 0.600 mg/cm²Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
[ISO 868
Hardness, Shore D 30
30
ISO 868
Tensile Strength at Break 17.0 MPa
2470 psi
ASTM D638
Elongation at Break 540 %
540 %
ASTM D638
Tensile Modulus 0.00610 GPa
0.885 ksi
ISO 527-2
Electrical Properties Metric English Comments
Volume Resistivity 2.70e+15 ohm-cm

@Temperature 90.0 °C
2.70e+15 ohm-cm

@Temperature 194 °F
ASTM D257
4.10e+15 ohm-cm

@Temperature 20.0 °C
4.10e+15 ohm-cm

@Temperature 68.0 °F
ASTM D257
Dielectric Constant 2.3

@Frequency 1000 Hz
2.3

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 35.0 kV/mm
889 kV/in
ASTM D149
Dissipation Factor 0.00060

@Frequency 1000 Hz
0.00060

@Frequency 1000 Hz
ASTM D150
Processing Properties Metric English Comments
Zone 1 140 - 160 °C
284 - 320 °F
Zone 2 150 - 170 °C
302 - 338 °F
Zone 3 160 - 180 °C
320 - 356 °F
Zone 4 160 - 180 °C
320 - 356 °F
Die Cooling Temperature 180 - 230 °C
356 - 446 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
RoHS Compliance RoHS Compliant