Nihon Superior SN97C Lead-Free Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Nihon Superior
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nihon Superior SN97C Lead-Free Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermal Properties Metric English Comments
Melting Point 218 - 219 °C
424 - 426 °F
Solidus 218 °C
424 °F
Liquidus 219 °C
426 °F
Component Elements Properties Metric English Comments
Copper, Cu 0.50 %
0.50 %
Silver, Ag 3.0 %
3.0 %
Tin, Sn 96.5 %
96.5 %
As Remainder