| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler |
| Manufacturer | Niche Polymer |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Niche Polymer PPHG20BK Homopolymer PP, 20% Glass Fiber Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.00500 cm/cm | 0.00500 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
| Elongation at Break | 2.00 - 3.00 % | 2.00 - 3.00 % | ASTM D638 |
| Flexural Strength | 86.2 MPa | 12500 psi | ASTM D790 |
| Flexural Modulus | 4.34 GPa | 630 ksi | ASTM D790 |
| Izod Impact, Unnotched | 0.747 J/cm <br>@Thickness 3.17 mm |
1.40 ft-lb/in <br>@Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 145 °C | 293 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 171 - 193 °C | 340 - 379 °F | ASTM D789 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Black |