Material Notes:
Description: NGAC P907-26 is a low viscosity and room temperature curing adhesive specifically formulated for optical applications where clarity is critical.Advantages and Applications: Uses include the assembly of optical components including the bonding of prisms and lenses. NGAC P907-26 is a low viscosity mixture that ensures exceptional wicking and wetting, along with superior adhesion strength to glass and plastic.Information Provided by Nextgen Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
Solids Content 100 %
100 %
Viscosity 600 cP
600 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Optical Properties Metric English Comments
Refractive Index 1.52
1.52
Processing Properties Metric English Comments
Cure Time 120 - 240 min

@Temperature 65.0 °C
2.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 40 - 50 min
40 - 50 min
Descriptive Properties Value Comments
Color Clear
Mix Ratio by Weight (R/H) 100/50