Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers NPP 25-0803

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP 25-0803.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Yield 23.8 MPa
3450 psi
2 in per min; ASTM D638
Elongation at Yield 14.5 %
14.5 %
chs 2 in/min; ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Gardner Impact 22.6 J

@Temperature -30.0 °C
16.7 ft-lb

@Temperature -22.0 °F
Gardner
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Users viewing this material also viewed the following: