Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NatureWorks® Ingeo™ 7001D ISBM Bottle Grade Biopolymer

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polylactic Acid (PLA) Biopolymer
Manufacturer NatureWorks LLC
Trade Name Ingeo™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NatureWorks® Ingeo™ 7001D ISBM Bottle Grade Biopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ingeo biopolymer 7001D is a thermoplastic resin derived from annually renewable resources and is specifically designed for use in injection stretch blow molded (ISBM) bottle applications. Ingeo biopolymer 7001D can be run using conventional ISBM equipment, but processes at lower temperatures than PET and can attain good resolution of mold detail on conventional tooling.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D1505
Moisture Vapor Transmission 13.8 - 15.7 cc-mm/m²-24hr-atm
35.1 - 39.9 cc-mil/100 in²-24hr-atm
ASTM F1249
Oxygen Transmission 25.6 - 27.6 cc-mm/m²-24hr-atm
65.0 - 70.1 cc-mil/100 in²-24hr-atm
ASTM D3985
Carbon Dioxide Transmission 106 - 118 cc-mm/m²-24hr-atm
269 - 300 cc-mil/100 in²-24hr-atm
NatureWorks test
Viscosity Measurement 4.0

@Temperature 30.0 °C
4.0

@Temperature 86.0 °F
Relative viscosity; 1.0 g/dl chloroform
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 210 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 410 °F
Thermal Properties Metric English Comments
Melting Point 145 - 160 °C
293 - 320 °F
ASTM D3418
Glass Transition Temp, Tg 55.0 - 60.0 °C
131 - 140 °F
ASTM D3418
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Transparent; thickness not specified