Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nanocyl PLASTICYL™ PP2001 Polypropylene with 2 wt% Multi-Wall Carbon Nanotubes

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Carbon Fiber Filled
Manufacturer Nanocyl
Trade Name PLASTICYL™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nanocyl PLASTICYL™ PP2001 Polypropylene with 2 wt% Multi-Wall Carbon Nanotubes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ PP2001 is a conductive masterbatch based on polypropylene. Because of its low viscosity and high flow formulation, PLASTICYL™ PP2001 is ideal for standard injection molding and extrusion processes.Key Applications:ESD (Electrostatic Discharge) and electrically conductive partsE&E automotive and industrialInjection molding, extrusionBenefits:Electrical conductivity at low loadingRetention of key mechanical propertiesEasier processing
Physical Properties Metric English Comments
Filler Content 2 %
2 %
Carbon Nanotube Loading
Melt Flow 5.6 g/10 min
5.6 g/10 min
ISO 1133:1997
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.5 MPa
5150 psi
ISO 527-1,2
Elongation at Break 154 %
154 %
ISO 527-1,2
Tensile Modulus 1.728 GPa
250.6 ksi
ISO 527-1,2
Charpy Impact, Notched 0.320 J/cm²
1.52 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Masterbatch; ISO 11357-1,-3
Electrical Properties Metric English Comments
Volume Resistivity 4.10e+6 ohm-cm
4.10e+6 ohm-cm
CTM E043
Surface Resistivity per Square 6.10e+10 ohm
6.10e+10 ohm
CTM E042
Copyright © lookpolymers.com All Rights Reserved