Material Notes:
High temperature, high strength general purpose stainless steel and other inert metals. For metal fittings
Physical Properties Metric English Comments
Viscosity 350000 - 550000 cP
350000 - 550000 cP
Paste
Mechanical Properties Metric English Comments
Shear Strength >= 68.9 MPa
>= 10000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
With Primer (Fixture)
240 min
4.00 hour
On steel (fixture)
1440 min
24.0 hour
On Steel (Full)
1440 min
24.0 hour
With Primer (Full)
Descriptive Properties Value Comments