Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NCMT NanoPAC™ HG602 High Performance Polypropylene Nanocomposite

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Nano Composite Materials Technology Ltd
Trade Name NanoPAC™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NCMT NanoPAC™ HG602 High Performance Polypropylene Nanocomposite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Household Industry Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
NCMT Method
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 27.0 MPa
3920 psi
ASTM D638
Elongation at Break <= 70 %
<= 70 %
ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM D638
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Deflection Temp.; ASTM D648
Users viewing this material also viewed the following: