Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mytex Polymers AS65K-2ATM Polypropylene, Talc filled, Compounded

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Mytex Polymers
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Mytex Polymers AS65K-2ATM Polypropylene, Talc filled, Compounded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology. This material exhibits high flow and good processability characteristics.Key Applications: Non-painted instrument panelInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Melt Flow 18 g/10 min
18 g/10 min
ASTM D1238
Ash 25 %
25 %
ASTM D5630
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
15 sec; ISO 868
Tensile Strength, Yield 20.0 MPa
2900 psi
50 mm/min; ISO 527
Flexural Modulus 2.17 GPa
315 ksi
Tangent; 1.3 mm/min; ISO 178
Izod Impact, Notched (ISO) 35.0 kJ/m²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ISO 75-1