Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 7000PL Photoluminescent Film

Category Polymer , Film
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7000PL Photoluminescent Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M Photoluminscent Film 7000PL is a high performance photoluminescent for film for safety and emergency exit signage. Meets and exceeds ASTM E207210, IMO A.752, OSHA 1910, 2000 IBC, DIN-67510 Part 4Rechargeable “glow in the dark” signs and markingsDimensionally stable, durable, multilayer filmExcellent chemical and stain resistanceEasily cleaned with 3M citrus Base CleanerNo radioactive materials used in manufacture of this productMay be safely disposed of in a sanitary landfill or by incinerationMay be imaged using 3M Scotchcal Screen Printing Inks 1900 and 9800 or thermal transfer methodsInformation provided by 3M
Physical Properties Metric English Comments
Thickness 229 - 279 microns
9.00 - 11.0 mil
film and adhesive
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 38.0 °C
100 °F
Application
90.0 °C
194 °F
Service
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Service
10.0 °C
50.0 °F
Application
Descriptive Properties Value Comments
Appearance Glossy appearance, light yellow green color
Users viewing this material also viewed the following: