Silberline Sparkle Silver® 5745

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name Sparkle Silver®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Sparkle Silver® 5745.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Sparkle Silver® 5745 is a fine, regular purity, non-leafing aluminum pigment with good opacity for solvent-based general industrial coatings. It provides excellent distinctiveness of image (D.O.I.) and brightness.Applications: Automotive; General Industrial
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
Bulk Factor 0.082
0.082
Volatiles 36 %
36 %
Particle Size 19 µm
19 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
0.01% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits/High Flash