Material Notes:
Multi-Pro 5002 X White is an extrusion grade filled polypropylene that has good stiffness as well as excellent impact properties. It can be made in any color.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792-91
Melt Flow 2.0 g/10 min
2.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 18.3 MPa
2650 psi
ASTM D638-95
Elongation at Break 500 %
500 %
ASTM D638-95
Flexural Modulus 2.241 GPa
325.0 ksi
ASTM D790-95
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D256-93a
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420-93