Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Misumi DC53 JIS Tool Steel

Category Metal , Ferrous Metal , Tool Steel , Cold Work Steel , Mold Steel
Manufacturer Misumi
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Misumi DC53 JIS Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose cold work die and mold steel whose strength and toughness approach those of high speed steels. Good machinability and grindability. Tougher than D2 Tool Steel. Machines 30% faster than D2 and A2. About the same strength as D2 Tool Steel after low-temperature tempering.Information provided by MISUMI Corporation.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 58.0 - 63.0
58.0 - 63.0
Thermal Properties Metric English Comments
CTE, linear 12.2 µm/m-°C

@Temperature 20.0 - 100 °C
6.78 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Processing Temperature 180 - 200 °C
356 - 392 °F
Tempered and air cooled
1020 - 1050 °C
1870 - 1920 °F
Hardened then air cooled
Users viewing this material also viewed the following: