Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Resin Type: linear copolymerCharacteristics: excellent physical properties, medium molecular weight distribution, wide range of processing conditions, good flow for injection blow molding applications, good parison uniformity, good trimability. Federal specification LP390C Classification Type I, Class H, Grades (1-5), Category 5. Meets FDA Regulation 21CFR 177.1520. Some restrictions apply when containing an antistatic additive.Applications: household and industrial chemicals, food packaging, personal care products, coolers, ice chests, sheet and vacuum forming, oil bottlesBurn rate < 5 cm/min.Information provided by Chevron Phillips Chemical Company.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
Apparent Bulk Density 0.590 g/cc
0.0213 lb/in³
ASTM D1895
Melt Flow 0.32 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.32 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength, Yield 29.6 MPa
4290 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
1% Secant; ASTM D 790
Tensile Impact Strength 95.0 kJ/m²
45.2 ft-lb/in²
S bar; ASTM D 1822
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D746
Users viewing this material also viewed the following: