Microtherm Group Slim&Light Fire Resistant Insulation

Category Ceramic , Oxide , Silicon Oxide , Other Engineering Material
Manufacturer Microtherm Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Microtherm Group Slim&Light Fire Resistant Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Microtherm® Slim&Light is a thin lightweight panel of ultra - high performance microporous thermal insulation. It is a highly efficient barrier to flame and heat. Microtherm® Slim&Light allows the design and fast assembly of thin, high efficiency lift fire doors. In a fire, stay cool with guaranteed fire security from Microtherm®.BenefitsMicrotherm® Slim&Light is available as a single large panel - no heat leakage through butt joints.This single fire resistant panel also aids fast, simple door assembly.The fire stopping efficiency of Microtherm® ensures the thinnest and lightest door construction.Microtherm® Slim&Light is non-combustible.Microtherm® Slim&Light is environmentally friendly with no respirable fibers.Comfortably maintains thermal performance and integrity through full 2 hour fire exposure on lift doors. Panels available for A60, A90, and A120 ratings. Enables thermal performance compliance to buildings/fire door regulations EN 1363-1 and EN 1364-1. Testing to EN 81-58:2003 “Fire resistance testing of lift landing doors”.Information provided by Microtherm.
Physical Properties Metric English Comments
Thickness 15000 - 30000 microns
591 - 1180 mil
according to rating
Thermal Properties Metric English Comments
Specific Heat Capacity 0.680 J/g-°C

@Temperature 0.000 °C
0.163 BTU/lb-°F

@Temperature 32.0 °F
0.920 J/g-°C

@Temperature 200 °C
0.220 BTU/lb-°F

@Temperature 392 °F
1.00 J/g-°C

@Temperature 400 °C
0.239 BTU/lb-°F

@Temperature 752 °F
Thermal Conductivity 0.0225 W/m-K

@Temperature 100 °C
0.156 BTU-in/hr-ft²-°F

@Temperature 212 °F
@ 320 kg/m³; estimated from plot
0.0250 W/m-K

@Temperature 500 °C
0.174 BTU-in/hr-ft²-°F

@Temperature 932 °F
@ 320 kg/m³; estimated from plot
0.0300 W/m-K

@Temperature 625 °C
0.208 BTU-in/hr-ft²-°F

@Temperature 1160 °F
@ 320 kg/m³; estimated from plot
0.0350 W/m-K

@Temperature 800 °C
0.243 BTU-in/hr-ft²-°F

@Temperature 1470 °F
@ 320 kg/m³; estimated from plot