MF-5040 Polyurethane-based Biomedical Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MF-5040 Polyurethane-based Biomedical Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D412
Tensile Strength, Yield 2.07 MPa
300 psi
at 100%; ASTM D412
Elongation at Break 700 %
700 %
ASTM D412