Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Microcell Composite Company CELLOMER® 3000 SBS Rubber Pellets

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Microcell Composite Company
Trade Name CELLOMER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Microcell Composite Company CELLOMER® 3000 SBS Rubber Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CELLOMER® PELLETS can be used in hot-pressing or with injection foaming boards. Featuring anti-slippage and elasticity.Information provided by Microcell Composite Company
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
Melt Flow 15 g/10 min

@Load 5.00 kg,
Temperature 200 °C
15 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 54
54
Tensile Strength, Yield 8.24 MPa
1190 psi
Elongation at Yield 600 %
600 %
Tear Strength 44.1 kN/m
252 pli