Material Notes:
Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treated and locally hardened. Recommended for dies, punches, spinning mandrels and other hard wearing applications.General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.Information provided by Meehanite Marketing Association.
Physical Properties Metric English Comments
Specific Gravity 7.34 g/cc
7.34 g/cc
Mechanical Properties Metric English Comments
Hardness, Brinell 280 - 550
280 - 550
Nominal
Tensile Strength, Ultimate 345 - 448 MPa
50000 - 65000 psi
Tensile Strength, Yield 172 MPa
25000 psi
.01% permanent set
Modulus of Elasticity 152 GPa
22000 ksi
Modulus of Rupture 0.641 GPa
93.0 ksi
Compressive Strength 1380 MPa
200000 psi
Poissons Ratio 0.33
0.33
Fatigue Strength 207 MPa
30000 psi
Machinability 52 %
52 %
Dalcher
Shear Modulus 65.5 GPa
9500 ksi
Izod Impact Unnotched 40.7 - 54.2 J

@Diameter 20.3 mm
30.0 - 40.0 ft-lb

@Diameter 0.798 in
Thermal Properties Metric English Comments
CTE, linear 12.1 µm/m-°C

@Temperature 37.8 - 538 °C
6.75 µin/in-°F

@Temperature 100 - 1000 °F
Shrinkage 1.3 - 1.5 %
1.3 - 1.5 %