Master Bond EP30R Fiber Reinforced Two Component Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP30R Fiber Reinforced Two Component Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Master Bond Polymer Adhesive EP30R is a fiber reinforced, high viscosity, two component epoxy adhesive for general purpose structural bonding formulated to cure at room temperature or more rapidly at elevated temperatures, with a four (4) to one (1) mix ratio by weight. EP30R produces high strength bonds which are resistant to thermal cycling and chemicals including water, oil and most organic solvents, over the wide temperature range of -60°F to more than 250°F.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 93.3 °C
2.00 - 3.00 hour

@Temperature 200 °F
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Yellow; "B" Yellow
Mix Ratio By Weight 100/25
Set-Up Time, minutes 30-35
At Room Temperature
Viscosity Paste
Room Temperature