Material Notes:
Master Bond Polymer System EP21HT is a two component, room temperature curing epoxy adhesive, sealant and coating with high temperature resistance up to 400°F. EP21HT produces high strength, durable bonds that hold up well to thermal cycling and resist many chemicals including water, oils, fuels, acids, bases and salts.
Physical Properties Metric English Comments
Viscosity 50000 - 60000 cP

@Temperature 23.0 °C
50000 - 60000 cP

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
1440 - 2880 min

@Temperature 23.0 °C
24.0 - 48.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Code "A" Clear; "B" Amber
Mix Ratio By Weight 100/100
Set-Up Time, minutes 50-70
At Room Temperature