LyondellBasell Petrothene® NA960070 Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LyondellBasell Petrothene® NA960070 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good uniformity, ease of processing and good tensile strength. Regulatory StatusThe basic resin NA 960 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing NA 960 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.Physical PropertiesThese are typical values and not to be construed as specific product limits. Data obtained from film produced inThis product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
2:1 BUR; 25 mil die gap
Melt Flow 0.90 g/10 min
0.90 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.5 MPa
2100 psi
Data derived from type IV specimen, 75 mil plaque @ 20" min.; ASTM D638
Film Elongation at Break, MD 200 %
200 %
ASTM D882
Film Elongation at Break, TD 500 %
500 %
ASTM D882
Elongation at Break 660 %
660 %
Molded; ASTM D638
Elmendorf Tear Strength MD 300 g
300 g
ASTM D1922
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
Dart Drop Test 120 g
0.265 lb
F<sub>50</sub>; ASTM D1709
Film Tensile Strength at Break, MD 24.1 MPa
3500 psi
ASTM D882
Film Tensile Strength at Break, TD 16.5 MPa
2400 psi
ASTM D882
1% Secant Modulus, MD 200 MPa
29000 psi
ASTM D882
1% Secant Modulus, TD 234 MPa
34000 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 °C
198 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F
Descriptive Properties Value Comments
Antiblock Low
Slip Medium