Michelman® ThermaGloss® 420 Water based over print varnish

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name ThermaGloss®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® ThermaGloss® 420 Water based over print varnish.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Water based over print varnish.Usage: ThermaGloss® 420 is a high heat resistant overprint which imparts excellent gloss to preprinted liner board while eliminating picking and smearing of the inks through the hot plate section of the corrugator. ThermaGloss® 420 has a reduced angle of skid.Application Data: ThermaGloss® 420 is designed for application by flexo or gravure on a preprint press.Typical uses include: Retail packaging; POP displays; and Ink protectionFood Contact Information when manufactured in the USA: FDA: 175.105: Components of adhesives. 176.170: Components of paper and paperboard in contact with aqueous and fatty foods.(Restricted)176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.05 - 1.07 g/cc
1.05 - 1.07 g/cc
pH 8.5 - 9.5
8.5 - 9.5
Brookfield Viscosity 50 - 300 cP
50 - 300 cP
Spindle # 3, rpm 60
Viscosity Measurement 30 - 40
30 - 40
[sec], EZ cup, Cup # 2
Descriptive Properties Value Comments
Appearance Light tan liquid
Solids Type Polymer