| Category | Fluid , Solvent |
| Manufacturer | LyondellBasell |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | LyondellBasell PMP Propylene glycol methyl ether propionate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.948 g/cc | 0.948 g/cc | 20/20°C |
| Density | 0.911 g/cc @Temperature 20.0 °C |
0.0329 lb/in³ @Temperature 68.0 °F |
|
| Solubility in Water | 6.1 % | 6.1 % | 20°C |
| Viscosity | 1.1 cP @Temperature 25.0 °C |
1.1 cP @Temperature 77.0 °F |
|
| Molecular Weight | 146 g/mol | 146 g/mol | |
| Vapor Pressure | 0.00120 bar @Temperature 20.0 °C |
0.900 torr @Temperature 68.0 °F |
|
| Evaporation Loss | 19 % | 19 % | n-BuAc=100% |
| Surface Tension | 34 dynes/cm | 34 dynes/cm | 25°C |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Boiling Point | 157 °C | 315 °F | at 760 mmHg |
| Flash Point | 56.0 °C | 133 °F | Tag Closed Cup |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.405 @Temperature 25.0 °C |
1.405 @Temperature 77.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| CAS Number | 148462-57-1 |