Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Microthene® G MN71400 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Microthene® G
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Microthene® G MN71400 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique properties of a polyolefin resin with a small ground particle size. Contact your Equistar sales and/or technical service representative for more information and specific recommendations for your application.Process TechniquesThe microfine size and irregular shape of Microthene G powders facilitate dispersibility with other components. Specific suggestions can be made only when equipment, materials, process parameters and conditions of use are known. Contact your Equistar technical representative for more information. Regulatory StatusMicrothene powders comply with certain Food and Drug Administration regulations, which may or may not permit their contact with food. Specific limitations or conditions of use may apply. Contact your Equistar Regulatory Affairs representative for more information. This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.912 g/cc
0.0329 lb/in³
ASTM D1505
Particle Mesh Size 50 Mesh
50 Mesh
Irregular shape. ETM = Equistar Test Method; ETM Malvern
Melt Flow 70 g/10 min
70 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 0.121 GPa
17.5 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 102 °C
216 °F
ASTM D3418
Vicat Softening Point 78.0 °C
172 °F
ASTM D1525
Brittleness Temperature -10.0 °C
14.0 °F
ASTM D746