Material Notes:
Silvaloy 2 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on vibration free joints. It is very effective for joining tight fittings and tubing. Silvaloy 2 is extremely fluid at brazing temperatures and will penetrate joints with very little clearance.Applications:The phosphorus content of Silvaloy 2 acts as a fluxing agent and no flux is necessary when brazing copper to copper joints. However, when used with a copper alloy or one of the other brazeable metals, a flux must be used to promote wetting, bonding, and flow throughout the joint. The flow point of Silvaloy 2 is 1300°F.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 8.00 g/cc
8.00 g/cc
Density 8.00 g/cc
0.289 lb/in³
Thermal Properties Metric English Comments
Melting Point 643 - 788 °C
1190 - 1450 °F
Solidus 643 °C
1190 °F
Liquidus 788 °C
1450 °F
Maximum Service Temperature, Air 149 °C
300 °F
continuous
204 °C
400 °F
intermittent
Component Elements Properties Metric English Comments
Copper, Cu 90.45 - 91.4 %
90.45 - 91.4 %
As balance
Other, total <= 0.15 %
<= 0.15 %
Phosphorous, P 6.8 - 7.2 %
6.8 - 7.2 %
Silver, Ag 1.8 - 2.2 %
1.8 - 2.2 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000315 ohm-cm
0.0000315 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 704 - 788 °C
1300 - 1450 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Light Copper
Electrical Conductivity (% IACS) 5.5