Material Notes:
Moplen RP342R is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP342R is a random copolymer particularly suitable for injection molding of houseware. Moplen RP342R meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520. And the components of additives are adequate on the food packaging substances specification of FDA regulation 21 CFR 178.2010.Features: Excellent Transparency; High gloss; Good flowability; Good mechanical property balanceApplications: Houseware; Food ContainerInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 31.4 MPa
4550 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.29 GPa
188 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Vicat Softening Point 135 °C
275 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 16 %
16 %