Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucas-Milhaupt HANDY HI-TEMP 870 High Temperature Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name HANDY HI-TEMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt HANDY HI-TEMP 870 High Temperature Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristics:Because of the wide melting range, this filler metal has good gap filling characteristics at the lower end of the brazing range and is relatively free-flowing near the upper end. Wetting is excellent on carbide stainless steel and copper. Recommended brazing clearances are .006"-.012". Fluxless braze in a vacuum or suitable protective atmosphere, or induction or furnace braze using Handy Hi-Temp M, Handy Hi-Temp DB or Handy Hi-Temp Boron Modified Flux. Applications:Handy Hi-Temp 870 is a bronze filler metal used for tungsten carbide to steel joints or stainless steels, requiring optimum high temperature shear strength, toughness and corrosion resistance. Brazing is often done in conjunction with heat treatment of the steel. Information provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Density 8.75 g/cc
0.316 lb/in³
Mechanical Properties Metric English Comments
Shear Strength 241 - 276 MPa
35000 - 40000 psi
Tungsten Carbide/ Tool Steel lap joints
Thermal Properties Metric English Comments
Melting Point 960 - 1029 °C
1760 - 1885 °F
Solidus 960 °C
1760 °F
Melting Point
Liquidus 1029 °C
1885 °F
Flow Point
Component Elements Properties Metric English Comments
Cobalt, Co 2.5 - 3.5 %
2.5 - 3.5 %
Copper, Cu 86 - 88 %
86 - 88 %
Manganese, Mn 9.0 - 11 %
9.0 - 11 %
Other, total <= 0.15 %
<= 0.15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000119 ohm-cm
0.0000119 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 1010 - 1090 °C
1850 - 2000 °F
Brazing Range
Descriptive Properties Value Comments
Color Light Copper