Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of LLP. Used where excellent optics and a tough, durable wrap are required. Ideal for low profile, long products. Strong seals and excellent shrinkage are obtained with all gauges. This is the fastest sealing linear low-density shrink film.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.630 cc-mm/m²-24hr-atm
1.60 cc-mil/100 in²-24hr-atm
ASTM 1249
Water Vapor Transmission 25.0 g/m²/day
1.61 g/100 in²/day
ASTM 1249
Oxygen Transmission 158 cc-mm/m²-24hr-atm
401 cc-mil/100 in²-24hr-atm
or 6300 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 160 %
160 %
Average; ASTM D882
Modulus of Elasticity 0.410 GPa
59.5 ksi
(stiffness), ASTM D882
Impact Test 1.60 J
1.18 ft-lb
Spencer Impact ASTM D3420
Coefficient of Friction, Dynamic 0.17
0.17
ASTM D1894
Elmendorf Tear Strength MD 40 g
40 g
Orientation not specified; ASTM D1922
Film Tensile Strength at Break, MD 103 MPa
14900 psi
ASTM D882
Optical Properties Metric English Comments
Haze 1.6 %
1.6 %
Gloss 140 %
140 %
Users viewing this material also viewed the following: