Mechanical Properties Metric English Comments
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
Huntsman KRYSTALFLEX® PE 501 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
SK Chemicals SKYTHANE® S195A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
Lubrizol Estane® 58246 Thermoplastic Polyurethane
Features: High stiffness grade with excellent chemical and oil resistance.Uses: Flat Die/Cast Film Extrusion and Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaI..
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
Lubrizol Estane® ALR E50D Thermoplastic Polyurethane
Type: Estane® ALR E50D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor..
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
Lubrizol Estane® AG 9550 Thermoplastic Polyurethane
Type: Estane® AG 9550 is a polyether based aliphatic polyurethane designed for flat die extrusion into film and sheet products.Features: Very tough, high modulus, high tear and tensile properties t..
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D638
Colorite Polymers 8500 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D638
Colorite Polymers 8502 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 02890 Plenum Flexible PVC
Non-lead stabilized PVC plenum jacket compound recommended for Category 5 applications. Good flexibility and handling during installation.Information provided by Georgia GulfGeorgia Gulf became Axi..
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 16881 Coax & Telecom Flexible PVC
90C rated, non-lead stabilized jacket compound with excellent low temperature properties. Suitable for riser and optical fiber constructions.Information provided by Georgia GulfGeorgia Gulf became ..
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 16882 Coax & Telecom Flexible PVC
Non-lead stabilized, 90C rated jacket compound with excellent low temperature properties. Formulated to be UV and fungal resistant. Suitable for riser and optical fiber constructions.Information p..
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 19900 Wire & Cable Flexible PVC
105°C; VW-1 rated non-lead stabilized insulation with good flexibility. Ideally suited for 1/64 wall (18 AWG and larger). UL approved for TW, THW, THHW applications.Information provided by Georgi..
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 2153 Wire & Cable Flexible PVC
THHN-THWN insulation for sizes 8 AWG and above. UL recognized for THHN, THW, THWN, TW, Oil resistant I.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 2153A Wire & Cable Flexible PVC
THHN-THWN; in circuit sizes (14 AWG and larger). UL recognized for THHN, THW, THWN, TW, Oil resistant I.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 22880 Coax & Telecom Flexible PVC
Flame retardant riser jacket over PVC or FR HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 7900 Moldings & Extrusions Flexible PVC
Clear, injection molding compound with good UV resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 8901 Moldings & Extrusions Flexible PVC
Outdoor grade extrusion compound formulated for good UV light resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 16900 Wire & Cable Flexible PVC
Tray cable jacket. 720 hour sunlight resistant in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 18853 Wire & Cable Flexible PVC
Non-lead stabilized 105°C rated jacket suitable for FT-4 applications over PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D412-80
DuPont Performance Polymers Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (discon
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
DuPont Performance Polymers Kalrez® 1050LF FFKM Perfluoroelastomer
A general-purpose compound for O-rings, seals, and other parts used in chemical process industries. It has good hot water/steam, excellent amine resistance, and enhanced compression set properties...
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 15900 Wire & Cable Flexible PVC
Non-lead stabilized insulation compound recommended for TW and 80C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Axiall 8918 Moldings & Extrusions Flexible PVC
Non-lead migration resistant extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Copyright © lookpolymers.com All Rights Reserved