Material Notes:
TPUs for Solvent-based adhesivesApplications: Shoe, OthersInformation provided by Merquinsa
Physical Properties Metric English Comments
Viscosity 1700 - 2100 cP
1700 - 2100 cP
15% solution in MEK
Processing Properties Metric English Comments
Processing Temperature 60.0 °C
140 °F
Min. Activation Temp; EN 12961
Descriptive Properties Value Comments
Crystallization Rate (MQSA n° 12 A) VERY HIGH
Solubility - Acetone / Ethyl Acetate 60:40
Solubility - Acetone / Toluene 65:35
Solubility - MEK / Toluene 75:25
Solubility - MEK/ Ethyl Acetate 75:25
Thermoplasticity Range (MQSA n° 58) MEDIUM