Multibase Multi-Flex® TPE A 8802 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 8802 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0108 cm/cm
0.0108 in/in
ASTM D955
Melt Flow 1.8 g/10 min
1.8 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
10 sec; ASTM D-2240
Tensile Strength, Ultimate 9.00 MPa
1310 psi
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
Flexural Modulus 0.00220 GPa
0.319 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 5.50 kN/m
31.4 pli
ASTM D624