Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials Pearlstick® 46-10/12 Polyester based TPU

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlstick®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlstick® 46-10/12 Polyester based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Pearlstick 46-10/12 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a high thermoplasticity level. Solubility: Pearlstick 46-10/12 is soluble in Methylene chloride, Acetone, Methyl Ethyl Ketone (MEK), Ethyl Acetate and Tetrahydrofurane (THF). Diluting solvents such as Toluene can be added in large amounts. The solvents and diluents should be water-free (max. 0.1 %), so as to avoid subsequent side reactions during crosslinking with isocyanate. It should be dissolved in closed tanks, and the use of a variable speed agitator is advisable. The final viscosity fies can vary, depending on the stirring process and on the solvent/diluents ratios Applications: Pearlstick 46-10/12 is used for the production of adhesives for plasticized PVC to plasticized PVC or other materials such as leather, textiles, metals, paper, etc. It can be used in the shoe industry as an adhesion promoter in the process of injection of PVC soles to the uppers Pearlstick 46-10/12 can be used as a two-component adhesive in furniture making, since two-component adhesives are advisable for the lamination of PVC films. The addition of a polyfunctional isocyanate to improves the heat-resistance and the strength of the joints.Information provided by Merquinsa
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 2781
Brookfield Viscosity 1000 - 1400 cP
1000 - 1400 cP
Brookfield RVF sp 3, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Processing Properties Metric English Comments
Processing Temperature 50.0 °C
122 °F
Min. Activation Temp; EN 12961
Descriptive Properties Value Comments
Crystallization Rate (MQSA n° 12 A) VERY HIGH
Hydroxyl Number 0.1%
MQSA 47A
Solubility - Acetone / Ethyl Acetate 0:100
Solubility - Acetone / Toluene 10:90
Solubility - MEK / Toluene 20:80
Solubility - MEK/ Ethyl Acetate 0:100
Thermoplasticity Range (MQSA n° 58) HIGH
Users viewing this material also viewed the following: