Oceanchem Group Melamine Polyphosphate (MPP)

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Melamine Polyphosphate (MPP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cas No.: 20208-95-1Use: Mainly used in polyamide and PBT, especially PA6, PA66, glass fiber-reinforced PA6, PA66. Nylon containing FR-NP can be used in all kinds of injection and extrusion processes and meets all processing demands of polyamide, glass fiber polyamide.FeaturesHalogen-free and low poison, meet European Environmental Protection requirementsEasy process, no need special screws combination and special specification glass fiberDifferent from general halogen retardant, no corrosion damage to equipment and moldGood het stability, decomposition temperature=330°C, suitable for glass fiber-reinforced nylonFlame retardant products containing FR-NP can be made to various colorStorage and Transportation: Handle with care, keep air-tight and dry.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Bulk Density 1.50 g/cc
0.0542 lb/in³
Density 1.60 g/cc
0.0578 lb/in³
Particle Size 25 µm
25 µm
Thermal Properties Metric English Comments
Decomposition Temperature 330 °C
626 °F
Component Elements Properties Metric English Comments
Phosphorous, P 15.01 %
15.01 %
Processing Properties Metric English Comments
Moisture Content 0.20 %
0.20 %
Descriptive Properties Value Comments
Appearance Fine, white, crystalline powder
CAS Number 20208-95-1