Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 175 - 190 °C
347 - 374 °F
Extrusion Molding
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane
ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon.
Zone 2 180 - 190 °C
356 - 374 °F
Injection
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 2 185 - 190 °C
365 - 374 °F
Equate EMDA-6200 HDPE Blow Molding Resin
EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for ..