Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 100 00V0 Polycarbonate, Flame Retardant

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Glass Fiber Filled, Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 100 00V0 Polycarbonate, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ASTM D683
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Tensile Modulus 2.20 GPa
319 ksi
ASTM D638
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 6.00 - 8.00 J/cm
11.2 - 15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 - 140 °C
275 - 284 °F
ASTM D1525, HDT Method B
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in