Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer CLAL-MSX
Trade Name DECLAFOR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turned partsInformation provided by CLAL-MSX
Physical Properties Metric English Comments
Density 8.80 g/cc
0.318 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 230 - 270
230 - 270
Tensile Strength, Ultimate 730 - 860 MPa
106000 - 125000 psi
Tensile Strength, Yield 630 - 780 MPa

@Strain 0.200 %
91400 - 113000 psi

@Strain 0.200 %
Elongation at Break >= 3.0 %
>= 3.0 %
Alo 100 mm
Modulus of Rigidity 115 GPa
16700 ksi
Torsion
Thermal Properties Metric English Comments
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
Thermal Conductivity 55.0 W/m-K
382 BTU-in/hr-ft²-°F
Melting Point 960 °C
1760 °F
Component Elements Properties Metric English Comments
Copper, Cu 87 %
87 %
Nickel, Ni 7.5 %
7.5 %
Other 0.50 %
0.50 %
Tin, Sn 5.0 %
5.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000130 ohm-cm
0.0000130 ohm-cm
Descriptive Properties Value Comments
Color Pinky roseate