Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase SILASTIC® C7-4565 TBPB Dow-Corning Biomedical Grade ETR Elastomer

Category Polymer , Thermoset , Silicone
Manufacturer Multibase
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase SILASTIC® C7-4565 TBPB Dow-Corning Biomedical Grade ETR Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Multibase
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
as molded
69
69
post cured- 2 hours at 177°C
75
75
post cured- 4 hours at 204°C
Tensile Strength, Ultimate 7.963 MPa
1155 psi
post cured- 4 hours at 204°C
8.27 MPa
1200 psi
post cured- 2 hours at 177°C
8.34 MPa
1210 psi
as molded
Tensile Strength, Yield 3.41 MPa
495 psi
at 200%, as molded
3.93 MPa
570 psi
at 200%, post cured- 2 hours at 177°C
4.31 MPa
625 psi
200%, post cured- 4 hours at 204°C
Elongation at Break 462 %
462 %
post cured- 4 hours at 204°C
533 %
533 %
post cured- 2 hours at 177°C
607 %
607 %
as molded
Tear Strength 32.1 kN/m
183 pli
post cured- 2 hours at 177°C; Die B
32.4 kN/m
185 pli
post cured- 4 hours at 204°C; Die B
38.7 kN/m
221 pli
as molded; Die B
Users viewing this material also viewed the following: