Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe Whitebear® Cold Work Tool Steel (ASTM A18)

Category Metal , Ferrous Metal , Alloy Steel , Tool Steel , Air-Hardening Steel , Cold Work Steel
Manufacturer Latrobe Steel
Trade Name Whitebear®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe Whitebear® Cold Work Tool Steel (ASTM A18).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Whitebear cold work tool steel is a versatile air-hardening tool steel in the 8% chromium family that is characterized by a very good combination of toughness and wear resistance. It contains lower carbon and total alloy content than most of the other cold work tool steels in the 8% chromium family, and these differences enhance the impact toughness of the steel at some sacrifice in wear resistance. Typical applications for Whitebear cold work tool steel include punches, blanking dies, thread roll dies, coining dies, drawing dies, upsetting dies, and rolls.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.81 g/cc
7.81 g/cc
Density 7.81 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 47
47
Air Cooled from 1066°C, 600°C Temper Temperature
59
59
Air Cooled from 1066°C, 149°C Temper Temperature
61
61
Air Cooled from 1066°C, 470°C Temper Temperature
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 65 - 70 %
65 - 70 %
1% Carbon Steel
Component Elements Properties Metric English Comments
Carbon, C 0.83 %
0.83 %
Chromium, Cr 7.75 %
7.75 %
Iron, Fe 86.37 %
86.37 %
Manganese, Mn 0.35 %
0.35 %
Molybdenum, Mo 1.55 %
1.55 %
Silicon, Si 1.0 %
1.0 %
Vanadium, V 2.15 %
2.15 %
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved