Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Monprene® MP 1257 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Teknor Apex Company
Trade Name MONPRENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Monprene® MP 1257 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: General Purpose; CSA Approved; OpaqueInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Melt Flow 10.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
ASTM D2240
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D412
Tensile Strength, Yield 1.72 MPa

@Strain 300 %
250 psi

@Strain 300 %
ASTM D412
Elongation at Break 770 %
770 %
ASTM D412
Users viewing this material also viewed the following: