A. Schulman POLYBATCH™ White LL8844 GP

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ White LL8844 GP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPOLYBATCH® LL8844 GP is a general purpose white color concentrate containing 45% TiO2 based in LLDPE. This product has been designed to provide color and opacity with good dispersion and distributive letdown mixing. POLYBATCH® LL8844 GP is typically recommended for use in polyethylene general purpose film, sheet, and injection molding applications. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.93 g/cc
1.93 g/cc
ASTM D792
Melt Flow 5.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 70 %
70 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789
Pellet Count 28
pellets/gram