Latrobe LSSâ„¢ 17-4 Precipitation Hardening Stainless Steel (ASTM Type 360)

Category Metal , Ferrous Metal , Martensitic , Stainless Steel , Precipitation Hardening Stainless
Manufacturer Latrobe Steel
Trade Name LSS™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe LSSâ„¢ 17-4 Precipitation Hardening Stainless Steel (ASTM Type 360).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TLS 17-4 is a precipitation hardening, martensitic stainless steel that exhibits excellent resistance to atmospheric and chemical corrosion. TLS 17-4 exhibits an excellent combination of high strength and corrosion resistance. Because it resists attack from the corrosive vapors that are produced during molding of some plastic resins, it is used extensively in nozzle tips and feed screws in the plastic injection molding industry. The corrosion resistance also enhances extended tool storage in humid environments. Other common applications include plastic mold cavity inserts, plastic extrusion dies, fasteners, valves, and gears. Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.80 g/cc
7.80 g/cc
Density 7.81 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 33
33
615°C Aging Temperature
44
44
480°C Aging Temperature
Modulus of Elasticity 197 GPa
28500 ksi
Poissons Ratio 0.272
0.272
Shear Modulus 77.4 GPa
11200 ksi
Calculated
Charpy Impact 6.00 J
4.43 ft-lb
480°C Aging Temperature
65.0 J
47.9 ft-lb
Thermal Properties Metric English Comments
CTE, linear 10.78 µm/m-°C

@Temperature 21.0 - 204 °C
5.989 µin/in-°F

@Temperature 69.8 - 399 °F
11.32 µm/m-°C

@Temperature 21.0 - 427 °C
6.289 µin/in-°F

@Temperature 69.8 - 801 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F

@Temperature 32.0 - 212 °F
Thermal Conductivity 17.87 W/m-K

@Temperature 149 °C
124.0 BTU-in/hr-ft²-°F

@Temperature 300 °F
19.46 W/m-K

@Temperature 260 °C
135.1 BTU-in/hr-ft²-°F

@Temperature 500 °F
22.62 W/m-K

@Temperature 482 °C
157.0 BTU-in/hr-ft²-°F

@Temperature 900 °F
Component Elements Properties Metric English Comments
Carbon, C 0.030 %
0.030 %
Chromium, Cr 15.75 %
15.75 %
Copper, Cu 3.5 %
3.5 %
Iron, Fe 74.37 %
74.37 %
Manganese, Mn 0.70 %
0.70 %
Nb + Ta 0.30 %
0.30 %
Nickel, Ni 4.75 %
4.75 %
Silicon, Si 0.60 %
0.60 %